The potential of utilization of alder wood fibers In medium density fiberboard production

In this investigation, 36 laboratory medium density fiberboard (MDF) panels were produced using Alder wood fibers. Variables factors were steaming time ( 5, 10 and 15 minutes), press time (4 and 6 minutes) and resin consumption (9 and 11%). The physical and mechanical properties of panels were measu...