The potential of utilization of alder wood fibers In medium density fiberboard production

In this investigation, 36 laboratory medium density fiberboard (MDF) panels were produced using Alder wood fibers. Variables factors were steaming time ( 5, 10 and 15 minutes), press time (4 and 6 minutes) and resin consumption (9 and 11%). The physical and mechanical properties of panels were measu...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Abolfazl Kargarfard, Amir Nourbakhsh, Fardad Golbabaei
Formato: article
Lenguaje:FA
Publicado: Regional Information Center for Science and Technology (RICeST) 2010
Materias:
Acceso en línea:https://doaj.org/article/239d608de59d403b9c1da0ca39291358
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
id oai:doaj.org-article:239d608de59d403b9c1da0ca39291358
record_format dspace
spelling oai:doaj.org-article:239d608de59d403b9c1da0ca392913582021-12-02T07:43:05ZThe potential of utilization of alder wood fibers In medium density fiberboard production1735-09132383-112X10.22092/ijwpr.2010.117261https://doaj.org/article/239d608de59d403b9c1da0ca392913582010-03-01T00:00:00Zhttp://ijwpr.areeo.ac.ir/article_117261_d41d8cd98f00b204e9800998ecf8427e.pdfhttps://doaj.org/toc/1735-0913https://doaj.org/toc/2383-112XIn this investigation, 36 laboratory medium density fiberboard (MDF) panels were produced using Alder wood fibers. Variables factors were steaming time ( 5, 10 and 15 minutes), press time (4 and 6 minutes) and resin consumption (9 and 11%). The physical and mechanical properties of panels were measured and analyzed. The results indicated that the maximum MOR was observed panels produced applying 6 minutes press time and resin consumption of 11%. The maximum Internal Bonding (IB) was related to panels made employing steaming time of 15 minutes and resin consumption of 11%. However, test panels produced at 6 minutes press time showed minimum of thickness swelling. The results indicated that the MDF boards produced from alder wood fibers exhibit desirable physical & mechanical properties were above than EN standard requirement. Consequently application of alder wood fibers to improve physical & mechanical properties of MDF panels which are produced from nonwood materials and agricaltural residues is recommended.Abolfazl KargarfardAmir NourbakhshFardad GolbabaeiRegional Information Center for Science and Technology (RICeST)articleMEDIUM DENSITY FIBERBOARDsteaming timePRESS TEMPERATUREPRESS TIMEPhysical & Mechanical PropertiesForestrySD1-669.5FAتحقیقات علوم چوب و کاغذ ایران, Vol 26, Iss 1, Pp 26-38 (2010)
institution DOAJ
collection DOAJ
language FA
topic MEDIUM DENSITY FIBERBOARD
steaming time
PRESS TEMPERATURE
PRESS TIME
Physical & Mechanical Properties
Forestry
SD1-669.5
spellingShingle MEDIUM DENSITY FIBERBOARD
steaming time
PRESS TEMPERATURE
PRESS TIME
Physical & Mechanical Properties
Forestry
SD1-669.5
Abolfazl Kargarfard
Amir Nourbakhsh
Fardad Golbabaei
The potential of utilization of alder wood fibers In medium density fiberboard production
description In this investigation, 36 laboratory medium density fiberboard (MDF) panels were produced using Alder wood fibers. Variables factors were steaming time ( 5, 10 and 15 minutes), press time (4 and 6 minutes) and resin consumption (9 and 11%). The physical and mechanical properties of panels were measured and analyzed. The results indicated that the maximum MOR was observed panels produced applying 6 minutes press time and resin consumption of 11%. The maximum Internal Bonding (IB) was related to panels made employing steaming time of 15 minutes and resin consumption of 11%. However, test panels produced at 6 minutes press time showed minimum of thickness swelling. The results indicated that the MDF boards produced from alder wood fibers exhibit desirable physical & mechanical properties were above than EN standard requirement. Consequently application of alder wood fibers to improve physical & mechanical properties of MDF panels which are produced from nonwood materials and agricaltural residues is recommended.
format article
author Abolfazl Kargarfard
Amir Nourbakhsh
Fardad Golbabaei
author_facet Abolfazl Kargarfard
Amir Nourbakhsh
Fardad Golbabaei
author_sort Abolfazl Kargarfard
title The potential of utilization of alder wood fibers In medium density fiberboard production
title_short The potential of utilization of alder wood fibers In medium density fiberboard production
title_full The potential of utilization of alder wood fibers In medium density fiberboard production
title_fullStr The potential of utilization of alder wood fibers In medium density fiberboard production
title_full_unstemmed The potential of utilization of alder wood fibers In medium density fiberboard production
title_sort potential of utilization of alder wood fibers in medium density fiberboard production
publisher Regional Information Center for Science and Technology (RICeST)
publishDate 2010
url https://doaj.org/article/239d608de59d403b9c1da0ca39291358
work_keys_str_mv AT abolfazlkargarfard thepotentialofutilizationofalderwoodfibersinmediumdensityfiberboardproduction
AT amirnourbakhsh thepotentialofutilizationofalderwoodfibersinmediumdensityfiberboardproduction
AT fardadgolbabaei thepotentialofutilizationofalderwoodfibersinmediumdensityfiberboardproduction
AT abolfazlkargarfard potentialofutilizationofalderwoodfibersinmediumdensityfiberboardproduction
AT amirnourbakhsh potentialofutilizationofalderwoodfibersinmediumdensityfiberboardproduction
AT fardadgolbabaei potentialofutilizationofalderwoodfibersinmediumdensityfiberboardproduction
_version_ 1718399207214153728