Thermopower peculiarities in thin bismuth wires
The resistance and thermoelectric power of pure bismuth wires are measured in longitudinal magnetic fields up to B = 14 T at temperatures between 4.2 and 25 K. At B = 0, the 200-nm samples exhibit large values of thermopower, which are dominated by diffusion with no phonon drag being evident. Both t...