Analysis of localized oxides and oxide films formed on alloy 625 and 617 in supercritical water and superheated steam environments at 750°C
Oxidation tests using coupon specimens of alloy 625 and alloy 617, and four-point bending tests for a duration of 100 hrs were carried out in supercritical water (SCW) environment at a pressure of 24 MPa and in superheated steam (SHS) environments at 750°C. The noticeable difference between the oxid...