Analysis of localized oxides and oxide films formed on alloy 625 and 617 in supercritical water and superheated steam environments at 750°C
Oxidation tests using coupon specimens of alloy 625 and alloy 617, and four-point bending tests for a duration of 100 hrs were carried out in supercritical water (SCW) environment at a pressure of 24 MPa and in superheated steam (SHS) environments at 750°C. The noticeable difference between the oxid...
Guardado en:
Autores principales: | Tatsuya ISHIKAWA, Yuji OZAWA, Masashi SAITO, Susumu NAKANO, Yoichi TAKEDA |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
The Japan Society of Mechanical Engineers
2017
|
Materias: | |
Acceso en línea: | https://doaj.org/article/3377886b00704474b275813106429a4e |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
The Strength of Inconel 625, Manufactured by the Method of Direct Laser Deposition under Sub-Microsecond Load Duration
por: Vladimir Promakhov, et al.
Publicado: (2021) -
The Journal of supercritical fluids
Publicado: (1988) -
Functional Materials for Waste-to-Energy Processes in Supercritical Water
por: Florentina Maxim, et al.
Publicado: (2021) -
El delito de violación en la ley 19.617
por: Valenzuela Mellado, Dina R
Publicado: (2000) -
Microstructure and Oxidation Behavior of Nb-Si-Based Alloys for Ultrahigh Temperature Applications: A Comprehensive Review
por: Fuqiang Shen, et al.
Publicado: (2021)