Corrosion of N10276 in a H<sub>2</sub>S, HCl, and CO<sub>2</sub> Containing Atmosphere at 480 °C and 680 °C

In several industrial processes, metallic materials suffer from chlorine- and sulfur-induced high-temperature corrosion. In previous studies, several steels have been tested at laboratory scale in a simulated gas atmosphere of a pyrolysis process of anthropogenic resources. In this paper, we propose...

Full description

Saved in:
Bibliographic Details
Main Authors: Manuela Nimmervoll, Gregor Mori, Edith Bucher, Alexander Schmid, Roland Haubner
Format: article
Language:EN
Published: MDPI AG 2021
Subjects:
HCl
Online Access:https://doaj.org/article/3f61d643f11c42dda8f4803aa5c9c051
Tags: Add Tag
No Tags, Be the first to tag this record!
Description
Summary:In several industrial processes, metallic materials suffer from chlorine- and sulfur-induced high-temperature corrosion. In previous studies, several steels have been tested at laboratory scale in a simulated gas atmosphere of a pyrolysis process of anthropogenic resources. In this paper, we propose a model on the course of corrosion in a H<sub>2</sub>S and HCl-containing atmosphere for N10276, which contains, besides iron, chromium, and nickel, also molybdenum as main alloying element. Bearing in mind the impact of the main alloying elements, as well as thermodynamic considerations and kinetic effects, the corrosion behavior of N10276 in a H<sub>2</sub>S and HCl-containing atmosphere at 480 °C and 680 °C can be explained. In addition, the corrosion behavior of N10276 is compared with earlier tested Fe-Cr-Ni alloys and differences in the corrosion behavior are stated within this paper.