Treatment of AMD using a combination of saw dust, bentonite clay and phosphate in the removal of turbid materials and toxic metals

Acid mine drainage collected from the western decant in South Africa was treated in a series of small-scale laboratory experiments. 200 mL of the sample was poured into five 500 mL glass beakers using flocculants formed by mixing size-optimized 1.5 g of bentonite clay with 3.5 g saw dust and 1.0 g o...