Quantitative dependence of ductile-to-brittle transition on phosphorus grain boundary segregation for a novel Ni–Cr–Mo RPV steel

SA508-4 N steel is considered a novel Ni–Cr–Mo low-alloy steel for reactor pressure vessels. The low-temperature embrittlement in the steel is an important issue that needs to be addressed. Herein, the main aim of this work is to investigate the non-hardening embrittlement caused by grain boundary s...