Thermoelectric properties of wires Bi-6at%Sb and Bi-8at%Sb under elastic stretches
Thin Bi1-xSbx wires with stibium concentration of 6 and 8at% in the free state and under elastic stretches are studied. Under 6-8% stretches the electron topological transition semiconductor-semimetal is found. The power factor is calculated.