Thermoelectric properties of wires Bi-6at%Sb and Bi-8at%Sb under elastic stretches
Thin Bi1-xSbx wires with stibium concentration of 6 and 8at% in the free state and under elastic stretches are studied. Under 6-8% stretches the electron topological transition semiconductor-semimetal is found. The power factor is calculated.
Guardado en:
Autor principal: | Popov, Ivan |
---|---|
Formato: | article |
Lenguaje: | EN |
Publicado: |
D.Ghitu Institute of Electronic Engineering and Nanotechnologies
2005
|
Materias: | |
Acceso en línea: | https://doaj.org/article/667f057ac6b84133b3fb2495a642a989 |
Etiquetas: |
Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
|
Ejemplares similares
-
Magnetothermoelectric properties of single-crystal wires and films based on Bi–3at%Sb
por: Nikolaeva, Albina, et al.
Publicado: (2019) -
Technology for preparation of thermal elements of SbBiTe alloys for thermoelectric coolers
por: Meglei, Dragoş, et al.
Publicado: (2005) -
BiSbO4 phase and its behavior under the action of light
por: Muntean, Ştefan, et al.
Publicado: (2009) -
Kinetic coefficients in Bi0.88Sb0.12 alloy: Influence of anisotropic deformation
por: Cherner, Iacov
Publicado: (2005) -
Thermoelectric effects in alloys Bi-Sn
por: Bodiul, Pavel, et al.
Publicado: (2006)