Analysis of mechanical and thermal stresses due to TiN coating of Fe substrate by physical vapor deposition

The residual stress generated after thin layer TiN coating by Physical Vapor Deposition is reducing the mechanical and tribological properties of TiN. Thermal stresses are one of the residual stress components which can cause failure modes of proper coatings. In this article, a validated computation...