Ductile and brittle behavior during deformation and fracture for pure ice detected by quasi-static indentation test

Ductile and brittle behavior during deformation and fracture for ice have attracted considerable research interest. The strength of ice has been reported to depend on the temperature, strain rate, and other factors. In addition, the tip shape of an object that comes into contact with ice is one of t...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Yuki NAKAO, Hiroyuki YAMADA, Nagahisa OGASAWARA, Takatoshi MATSUZAWA
Formato: article
Lenguaje:EN
Publicado: The Japan Society of Mechanical Engineers 2021
Materias:
ice
Acceso en línea:https://doaj.org/article/78253277828340408ffc15f3c88f10a5