Cutting Power during Milling of Thermally Modified Pine Wood
The paper presents experimental testing results of cutting power of thermally modified wood of Scots pine (Pinus sylvestris L.) during lengthwise milling. The process of heat treatment was performed in the atmosphere of superheated steam, at temperatures of 130, 160, 190 and 220 °C, maintaining an i...