Experimental Analysis on Behaviour of Adhesive Scale in Hot Die Forging to Improve Surface Quality of Automobile Parts

Deep dent defects on the automobile parts produced by hot die forging have become problems because the dents were disadvantageous to the strength of these parts. The dents may have been probably caused by scales of hot billets. The behaviour of these thick scales in hot die forging was experimentall...