Experimental Analysis on Behaviour of Adhesive Scale in Hot Die Forging to Improve Surface Quality of Automobile Parts
Deep dent defects on the automobile parts produced by hot die forging have become problems because the dents were disadvantageous to the strength of these parts. The dents may have been probably caused by scales of hot billets. The behaviour of these thick scales in hot die forging was experimentall...
Enregistré dans:
Auteurs principaux: | Kazuhiko Kitamura, Kazuhito Asai, Motoki Terano |
---|---|
Format: | article |
Langue: | EN |
Publié: |
Japanese Society of Tribologists
2014
|
Sujets: | |
Accès en ligne: | https://doaj.org/article/8912fd7dd1eb4f1dbd40ca7bd47e7426 |
Tags: |
Ajouter un tag
Pas de tags, Soyez le premier à ajouter un tag!
|
Documents similaires
-
Wear Analysis of Forging Tools Used in an Industrial Production Process—Hot Forging in Closed Dies of the “Head-Disk” of an Engine Valve Forging
par: Marek Hawryluk, et autres
Publié: (2021) -
Investigation of effective geometrical parameters on wear of hot forging die
par: Mohammadmahdi Davoudi, et autres
Publié: (2021) -
Prediction of the parameters and the hot open die elongation forging process on an 80 MN hydraulic press
par: Dindorf Ryszard, et autres
Publié: (2021) -
Upper Bound Analysis of Closed-Die Forging of Eccentrically-Located SiCp AMC Preforms
par: Manish Agarwal, et autres
Publié: (2021) -
Numerical Model Simulation of the Double-Roll Rotary Forging of Large Diameter Thin-Walled Disk
par: Zhongquan Yu, et autres
Publié: (2021)