Experimental Analysis on Behaviour of Adhesive Scale in Hot Die Forging to Improve Surface Quality of Automobile Parts
Deep dent defects on the automobile parts produced by hot die forging have become problems because the dents were disadvantageous to the strength of these parts. The dents may have been probably caused by scales of hot billets. The behaviour of these thick scales in hot die forging was experimentall...
Saved in:
Main Authors: | Kazuhiko Kitamura, Kazuhito Asai, Motoki Terano |
---|---|
Format: | article |
Language: | EN |
Published: |
Japanese Society of Tribologists
2014
|
Subjects: | |
Online Access: | https://doaj.org/article/8912fd7dd1eb4f1dbd40ca7bd47e7426 |
Tags: |
Add Tag
No Tags, Be the first to tag this record!
|
Similar Items
-
Wear Analysis of Forging Tools Used in an Industrial Production Process—Hot Forging in Closed Dies of the “Head-Disk” of an Engine Valve Forging
by: Marek Hawryluk, et al.
Published: (2021) -
Investigation of effective geometrical parameters on wear of hot forging die
by: Mohammadmahdi Davoudi, et al.
Published: (2021) -
Prediction of the parameters and the hot open die elongation forging process on an 80 MN hydraulic press
by: Dindorf Ryszard, et al.
Published: (2021) -
Upper Bound Analysis of Closed-Die Forging of Eccentrically-Located SiCp AMC Preforms
by: Manish Agarwal, et al.
Published: (2021) -
Numerical Model Simulation of the Double-Roll Rotary Forging of Large Diameter Thin-Walled Disk
by: Zhongquan Yu, et al.
Published: (2021)