The strengthening efficacy of filler/interphase network in polymer halloysite nanotubes system after mechanical percolation
A defective interphase section in polymer halloysite nanotubes (HNT) system is considered and the influences of required interfacial shear strength for effective stress conveying via interphase zone (τc) and interfacial shear strength (τc) on the effective interphase depth, effective filler amount a...