Properties of high quality paper from rag fibers recycling
In this investigation, soda pulps from old rags applying three pulping times (60, 120 and 180 minutes ) and three levels of active alkali ( 6,8, and 10% NaOH based on OD weight of rag) and pulping temperature of 125º C were produced. Liquor to rag ratio was kept constant at 11:1(based on the weight...