In this article, we present an experimental study on the impact of post-metallization annealing conditions on the negative-bias temperature instability (NBTI) of Si p-channel fin field-effect transistors (p-FinFETs) with atomic layer deposition tungsten (ALD W) as the gate-filling metal. The effects...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Longda Zhou, Qianqian Liu, Hong Yang, Zhigang Ji, Hao Xu, Guilei Wang, Eddy Simoen, Haojie Jiang, Ying Luo, Zhenzhen Kong, Guobin Bai, Jun Luo, Huaxiang Yin, Chao Zhao, Wenwu Wang
Formato: article
Lenguaje:EN
Publicado: IEEE 2021
Materias:
Acceso en línea:https://doaj.org/article/c5b752e8b8c341c8ae304cdcd783f0ac
Etiquetas: Agregar Etiqueta
Sin Etiquetas, Sea el primero en etiquetar este registro!
Descripción
Sumario:In this article, we present an experimental study on the impact of post-metallization annealing conditions on the negative-bias temperature instability (NBTI) of Si p-channel fin field-effect transistors (p-FinFETs) with atomic layer deposition tungsten (ALD W) as the gate-filling metal. The effects of annealing conditions on the tensile stress of the W film, impurity element concentration in the gate stack, fresh interface quality, threshold voltage shift (<inline-formula> <tex-math notation="LaTeX">${\Delta }$ </tex-math></inline-formula> <italic>V</italic><inline-formula> <tex-math notation="LaTeX">$_{T}$ </tex-math></inline-formula>), pre-existing traps (<inline-formula> <tex-math notation="LaTeX">${\Delta } {N} _{\mathrm {HT}}$ </tex-math></inline-formula>), generated traps, and their relative contributions were studied. The time exponents of <inline-formula> <tex-math notation="LaTeX">${\Delta }$ </tex-math></inline-formula> <italic>V</italic><inline-formula> <tex-math notation="LaTeX">$_{T}$ </tex-math></inline-formula>, the impacts of stress bias and temperature on NBTI degradation, and the recovery kinetics of the generated traps were analyzed. For devices with a B<sub>2</sub>H<sub>6</sub>-based W-filling metal, a 34&#x0025; reduction in the fresh interface states, reduced <inline-formula> <tex-math notation="LaTeX">${\Delta }$ </tex-math></inline-formula> <italic>V</italic><inline-formula> <tex-math notation="LaTeX">$_{T}$ </tex-math></inline-formula>, and a 29&#x0025; improvement in the operation overdrive voltage could be achieved by optimizing the annealing conditions. The NBTI is alleviated mainly because of the reduction in the generated traps, while the energy distribution of <inline-formula> <tex-math notation="LaTeX">${\Delta } {N} _{\mathrm {HT}}$ </tex-math></inline-formula> is insensitive to the annealing conditions. Furthermore, the relative contribution of the generated bulk insulator traps to the total number of generated traps could be reduced by optimizing the annealing conditions.