Preparation of ZnTe thin films using chemical bath deposition technique

Chemical bath deposition was used to prepare thin films of ZnTe. The density of compounds (0.5–2) ml in 50 ml of distilled water, the precipitation time (10–80 min), and the solution temperature during the precipitation process (15–85 °C) have been changed during the preparation of the ZnTe thin fil...