Optimized low-cycle fatigue behavior and fracture characteristics of Ti–6Al–4V alloy by Fe microalloying

In the present work, low cycle fatigue (LCF) behavior and fracture characteristic of Ti–6Al–4V-0.55Fe alloy with bimodal microstructure, consisted of equiaxed primary α (αp), lamellar α (αl) and β matrix, are systematically investigated at room temperature. Results indicate that Ti–6Al–4V-0.55Fe all...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Yangyang Sun, I.V. Alexandrov, Yuecheng Dong, R.Z. Valiev, Hui Chang, Lian Zhou
Formato: article
Lenguaje:EN
Publicado: Elsevier 2021
Materias:
Acceso en línea:https://doaj.org/article/d71073d3d42d4ce2941f00ee0f4130dd
Etiquetas: Agregar Etiqueta