Volcanic Tuff as Secondary Raw Material in the Production of Clay Bricks

The present work examines an innovative manufacturing technique for fired clay bricks, using tuff as a secondary raw material. Samples were made of clay and tuff (0–30 wt.%) fired at 900 to 1100 °C. The chemical and mineralogical compositions and physical and thermal analyses of raw materials were i...

Full description