Influence of high-energy ball milling on the optical transmittance and some mechanical and tribological properties of a bone china
Bone china samples were produced using two different milling methods: low-energy ball milling (LEBM) for 3 and 24 h, and high-energy ball milling (HEBM) for 5 min. After pressing, the samples were sintered at temperatures ranging from 1100 °C to 1250 °C. HEBM 5 min yields a raw materials’ specific s...